As an antifouling for boats of glass fibre, wood, plywood, steel and aluminium. For power boats and regatta yachts.
Price:
€133.04
Listing:
€211.18
You Save:
€78.14 (37%)

Description

Hempel Hard Racing TecCel Antfouling 2.5Lt 10000 White

HEMPEL’S HARD RACING TecCel 7688W is a high performance, hard antifouling providing
outstanding protection all season. Includes TecCel technology which ensures reduced friction and increased speed. As an antifouling for boats of glass fibre, wood, plywood, steel and aluminium. For power boats and regatta yachts.
PHYSICAL CONSTANTS:
Shade nos/Colours: 10000/ White.
Finish:Flat
Volume solids, %: 54 ± 1
Theoretical spreading rate: 13.5 m2/l [541.4 sq.ft./US gallon] - 40 micron/1.6 mils
VOC content: 404 g/l [3.4 lbs/US gallon]
Dry to touch: 4 hour(s) 20°C/68°F
                   8 hour(s) 10°C/50°F
Specific gravity: 1.4 kg/litre [11.4 lbs/US gallon]
Flash point: 35 °C [95 °F]
Shelf life: 5 years 25°C/77°F

APPLICATION DETAILS:
Application method: Brush/Roller/Paint pad
Spray: For professional use only.
Thinner (max.vol.): HEMPEL'S THINNER 808 (No 3) 08081 (Brush/Roller/Paint pad): max. 5%
HEMPEL'S THINNER 808 (No 3) 08081 (Spray): 5-15%
Nozzle orifice: 0.018 - 0.023 "
Nozzle pressure: 150 bar [2175 psi]
(Airless spray data are indicative and subject to adjustment)
Indicated film thickness, dry: 40 micron [1.6 mils]
Indicated film thickness, wet: 75 micron [3 mils]
Overcoat interval, min: 4 hour(s) 20°C/68°F
8 hour(s) 10°C/50°F
Overcoat interval, max: None

SURFACE PREPARATION:
Preparation: Always ensure all surfaces are clean, oil free and dry. Clean the surface and remove possible oil and grease with a suitable detergent and sand with dry abrasive paper. Carefully remove dust with fresh water.
Uncoated surface: Prime prepared surface with HEMPEL’S LIGHT PRIMER 45551 and apply a tiecoat of HEMPEL’S UNDERWATER PRIMER 26030 whilst the surface is still tacky.
Existing old self-polishing or traditional antifouling: Remove loose matter and contaminants by high pressure fresh water cleaning. Allow to dry.
Existing old hard matrix antifouling or an unknown antifouling:
High pressure fresh water clean, wet abrade, remove dust. Clean and dry the surface. If condition of previous antifouling is poor, seal with 1 coat of HEMPEL’S UNDERWATER PRIMER 26030. If previous antifouling is in general bad condition, it is recommended to remove previous coats and prime before applying antifouling.

PRODUCT APPLICATION: Method: Apply 2 coats of the Antifouling paint at 40 μm dry film thickness each. Apply an additional coat around the waterline and high wear areas. Add thinner to assist application if necessary: max. 5%.
Stir product well before use. Wear protective gloves/clothing and eye/face protection.

Colours/Colour stability: Final colour develops after 1 week immersion in water. Length of service may have a certain influence on colour. The antifouling may obtain a copper-green tinge. There might be a slight difference in colour from batch to batch. Mix before painting.

Packing 2.5L. White colour.